Base MaterialRogers/Taconic/Isola
Dielectric Constant2.2-10.2
Loss Tangent0.0009-0.003
Frequency Range1GHz-77GHz
Impedance Control±5%
Layers2-16 layers

Product Features

Rogers/Taconic/PTFE materials
Low dielectric loss
Stable Dk/Df values
5G/radar optimized
Mixed dielectric lamination
Tight impedance tolerance

Applications

5G Base Station Antennas
Radar Systems
Satellite Communications
Automotive Millimeter-Wave Radar
RF Modules
Microwave Communications

FAQ

Are you a high frequency PCB manufacturer?
Yes. Sunking PCB is a professional high frequency PCB manufacturer with our own factory, producing prototypes and volume orders on Rogers, Taconic and Isola materials, with Dk 2.2-10.2 covering 1GHz to 77GHz.
What materials and frequency range does your high frequency PCB manufacturing support?
Our high frequency PCB manufacturing supports Rogers 4350B/4003C, Taconic RF series, PTFE and mixed-dielectric lamination, with loss tangent as low as 0.0009 and ±5% impedance control for 5G, radar, satellite and millimeter-wave applications.
As a high frequency PCB factory and supplier, what are your lead time and MOQ?
As a high frequency PCB factory and supplier, prototypes ship in as fast as 5-7 working days from 5 pieces, with volume pricing on request; we stock Rogers and other imported materials to shorten lead time.

Need a quote for High Frequency PCB?

Upload your Gerber files and we'll provide a professional quote within 24 hours.

Get Quote Now