Key Products
-
sk164A182739
Type: 32-Pieces-Simple Panel
Format: 2L Copper substrate
Material: VT4B3
Surface: Chemical gold 2U
Min Track / Space: 100µm
Min. Drill Dia.: 0.1mm
Soldermask: Top + Bottom
Marking Print: White
E-Test: Yes
Sideplating: Yes
Burried Vias: Yes
Blind Vias: Yes
-
994A194356
Type: 32-Pieces-Simple Panel
Format: 2L Copper substrate
Material: VT4B3
Surface: Chemical gold 2U
Min Track / Space: 100µm
Min. Drill Dia.: 0.1mm
Soldermask: Top + Bottom
Marking Print: White
E-Test: Yes
Sideplating: Yes
Burried Vias: Yes
Blind Vias: Yes
-
PCB Manufacturing
Panel: 8019.01_0394271-01
Type: 15-Pieces-Simple Panel
Format: 8 - Layer - Multilayer
Surface:Chemical gold 2U
Mech. treatment:Milled with perf.bridges
Panel-Size: 172,80mm x 99,50mm = 1,72dm²
Material: FR4 Tg 150 S1000H 1.0mm OL:35µm / IL:35µm Cu
Min Track / Space:100µm
Min. Drill Dia:0.1mm
Soldermask: Top + Bottom, green
Marking Print: without
E-Test: Yes
Sideplating: Yes
Burried Vias: Yes
Blind Vias: Yes
-
PCB Manufacturing
Panel: 8019.01_0394271-01
Type: 15-Pieces-Simple Panel
Format: 8 - Layer - Multilayer
Surface:Chemical gold 2U
Mech. treatment:Milled with perf.bridges
Panel-Size: 172,80mm x 99,50mm = 1,72dm²
Material: FR4 Tg 150 S1000H 1.0mm OL:35µm / IL:35µm Cu
Min Track / Space:100µm
Min. Drill Dia:0.1mm
Soldermask: Top + Bottom, green
Marking Print: without
E-Test: Yes
Sideplating: Yes
Burried Vias: Yes
Blind Vias: Yes
-
Depth milling PCB
Type: 4 different kinds board in one simple Panel
Format: 2 Layer
Surface:Chemical gold 2U
Mech. treatment:Milled with perf.bridges
Material: FR4 Tg 150 S1000H 1.0mm OL:35µm / IL:35µm Cu
Min Track / Space:100µm
Min. Drill Dia:0.1mm
Soldermask: Top + Bottom, green
Marking Print: without
E-Test: Yes
Depth milling: Yes
-
Volkswagen LED board
Type: 4-Pieces-Simple Panel
Format: 2 - Layer - Multilayer
Surface: LF-HASL
Mech. treatment:Milled with perf.bridges
Material: FR4 TG 150 S1000H 1.0mm OL:35µm / IL:35µm Cu
Min Track / Space:100µm
Min. Drill Dia:0.1mm
Soldermask: Top + Bottom, green
Marking Print: White
E-Test: Yes