Sunking PCB

Ceramic Substrate Holes and Outlines: When They Are Formed Decides What You Can Draw

Design Guide2026-10-16Sunking Circuits Technical Team
Ceramic Substrate Holes and Outlines: When They Are Formed Decides What You Can Draw

The short version: on a ceramic substrate, holes and outlines are not a back-end operation. They are fixed much earlier in the process chain. Whether forming happens before or after sintering decides what governs hole-location accuracy, how good an edge you can get, and how many singulation options are left on the table.

1. Why "just drill a hole in the ceramic board" does not survive contact with the shop floor

In the FR-4 world the process order is almost automatic: laminate, drill, metallise, image, solder mask, surface finish, then rout the outline or V-cut the array. Holes and outlines sit near the end because the base material is tough enough — a drill enters, a router passes, and the material is removed in a predictable way.

Ceramic has none of that toughness. It is hard and brittle, and under concentrated load it does not deform, it cracks. Two consequences follow. First, mechanical drilling and routing are not default options on ceramic. Second, the "finish the board, then cut it" order is itself risky — the value of every preceding operation can be lost in a single chip-out at the last step.

So ceramic process routes push hole and outline forming earlier. Two mainstream approaches exist: forming while the ceramic is still green (unsintered), or machining after sintering using non-contact or abrasive methods. These are not two names for the same thing. They are two routes whose accuracy comes from entirely different sources.

The question this article answers is not "can ceramic take this hole." It can. The real question is: at which step is this hole and this edge created, what is the accuracy staked on, and which conclusions must wait for engineering review rather than being settled at design time. Which base material and metallisation to choose is a separate question — see alumina vs AlN and DPC vs DBC routes.

2. The two routes and what each stakes accuracy on

AspectGreen-stage formingPost-sinter machining
What is being formedSoft, unsintered ceramic sheetAlready sintered, hard and brittle substrate
Typical methodsPunching, die forming, piercing in the green stateLaser processing, diamond abrasive grinding or cutting
Accuracy governed primarily bySintering shrinkage — formed dimensions are oversized; final size is set by shrinkageThermal and abrasive damage — size is direct, but edge condition is set by the cutting process
Typical riskUneven shrinkage shifting or distorting the whole hole patternEdge chipping, micro-cracking, heat-affected material
Features it suitsHigh quantity, repeating, regular holes and outlinesOne-off or low volume, irregular shapes, features only defined after sintering
Cost of a changeRequires a new die or forming toolProgram change only, but longer time per piece

The row most often skipped is "accuracy governed primarily by." It means the same hole-location requirement is not the same difficulty on the two routes, and is not owned by the same step. When a designer writes a hole-location requirement without knowing which route the board takes, that requirement may land on a step that cannot carry it.

3. Green-stage forming: shrinkage governs hole location, so the datum has to follow

In the green state ceramic can be punched and pierced — this is the closest it ever gets to being easy to machine. The price arrives later: sintering shrinks the whole body.

Shrinkage is a whole-sheet behaviour, not a local error. In engineering terms: every formed dimension must be made oversized, and the oversize factor applies to the whole sheet. Hole-to-hole spacing and hole-to-edge distance therefore all move together. If shrinkage is not perfectly uniform across the sheet — and in real production that is the norm, not an anomaly — the deviation shows up as a systematic shift or distortion of the pattern, not as random error on one hole.

This creates one concrete design input: the hole-location datum must be declared. Whether a group of holes is referenced to the board edge or to a datum feature on the board makes little difference on FR-4. On a ceramic board taking the green-forming route, that choice decides how shrinkage deviation is distributed. Referenced to the edge, holes near the edge behave best and the centre region worst. Referenced to a central datum feature, deviation is shared toward both sides. Which is preferable depends on which holes matter most — information only the designer has, and the factory cannot decide on your behalf.

A second implication: regular repeating features are cheap, scattered features are not. Green forming depends on tooling, and tooling cost tracks how regular the features are. An array of identical holes and a set of individually placed irregular openings are not the same order of magnitude on this route.

4. Post-sinter machining: edge condition becomes something you must declare

After sintering the substrate is already at final size, so this route has no shrinkage problem — dimensions can be made directly. The problems are simply a different set.

Heat effects. Laser processing removes material through locally concentrated energy, so the edge of the processed zone inevitably sees a steep temperature change. Ceramic is sensitive to thermal stress, so a cut edge can be left with a layer whose properties differ from the bulk, plus micro-cracks that are not readily visible. These may not affect appearance at all when processing finishes, yet become crack initiation sites under later assembly stress or thermal cycling.

Edge chipping. Whether by laser or by abrasive grinding, ceramic edges fail by losing material, not by growing a burr. This is a different class of problem from deburring a routed FR-4 edge: a burr can be removed, a chip-out cannot — the material is already gone.

So edge condition cannot be left as a default. On an FR-4 drawing an outline edge usually carries only dimensions and tolerance, with edge condition covered by common practice. Doing the same on ceramic produces a predictable dispute: the factory ships to common practice, the customer rejects against assembly needs, and neither party is wrong — because the drawing never said what that edge has to do. If the edge will later mate to a heat sink surface, enter a fixture, or carry clamping load, that requirement belongs on the drawing, not in the conversation after rejection. For contrast, see PCB outline machining tolerance — and note that its conclusions do not transfer directly to ceramic.

5. Singulation: of the FR-4 toolkit, barely one and a half options survive

Three singulation methods are common on conventional base materials. Their viability on ceramic differs completely:

Singulation methodConventional base materialCeramic substrate
V-cut (score then snap)Common, low costEssentially unusable. Snapping a brittle material means the crack path is uncontrolled and the broken face cannot be guaranteed
Rout-out (cutting the tabs)CommonLimited. Mechanical routing on ceramic needs dedicated abrasive tooling, and the tab area is where chipping concentrates
PunchingUsed for high volume, regular shapesOnly viable in the green state. Punching after sintering means cracking the substrate
Laser separationLess commonOne of the main methods, accepting heat effects and longer time per piece

The direct consequence: array design cannot be copied over. On conventional material, panelisation balances material utilisation, ease of separation and shipping strength, and tab and V-cut placement follow established practice (see panel array design and process constraints and outline routing and V-cut tolerance). On ceramic, V-cut is struck off first, so whether an array makes sense has to be recalculated — and sometimes the answer is "no array, machine as single pieces," which in turn changes the quoting structure and the delivery format.

6. Who decides what

Sorting the conclusions above by ownership makes the boundary clear.

Inputs the designer must provide:

  • Which hole positions are critical, and what they are referenced to (this directly decides how shrinkage deviation is distributed)
  • What each outline edge has to do later (mating, fixture entry, load bearing, or appearance only)
  • Whether the board has features that can only be defined after sintering
  • Whether single-piece delivery is acceptable (this decides whether the array discussion is worth having at all)

Conclusions that must wait for engineering review and cannot be settled at design time:

  • Green-stage forming versus post-sinter machining — it depends on feature regularity, quantity and tooling feasibility
  • Achievable hole size and location capability — coupled to material, thickness and route, not a fixed number
  • How good an edge is achievable — tied directly to the route
  • The singulation method, and whether an array is viable at all

The benefit of drawing this line is direct: the designer stops guessing at factory capability, and the factory stops guessing which hole is the critical one. The SKPCB manufacturing capabilities overview and tolerance information state the published capability framing; a specific ceramic build still needs its own review against the inputs above. For category context see the ceramic substrate PCB guide and the ceramic PCB product page. If the real driver turns out to be heat spreading rather than the insulating substrate itself, metal core PCB may be the better direction.

7. What the drawing and data package need to add

Making this process order executable does not require much, but these items will always be asked for if missing:

  1. An explicit hole-location datum — not "per drawing," but a named datum feature or datum edge
  2. Identification of critical holes — which positions cannot move, while the rest follow the pattern
  3. A functional statement per outline edge — what each edge does later, or at minimum which edges are functional and which are not
  4. Edge condition requirements — if there is an assembly or mating need, state it; do not rely on common practice
  5. Acceptable delivery format — single pieces or array, and whether the factory may adjust for process feasibility
  6. Marking of post-processed features — which features may be machined after sintering and which must be formed integrally

None of these six is a numeric commitment. They are ownership statements. Their purpose is to let the first review round return a definite answer, instead of discovering a datum misunderstanding after the third sample build. For the published framing on inspection and release, see quality; for material-side published information, see materials.

FAQ

Q1: Can ceramic substrates be mechanically drilled at all?

Mechanical drilling is not a default method on ceramic. The material is hard and brittle, and concentrated drilling load readily causes cracking or entry/exit chipping. Practical routes are green-stage forming or post-sinter laser and abrasive machining. Whether a specific feature on a specific board can be handled mechanically is an engineering review item and cannot be assumed from FR-4 experience.

Q2: Why did the whole hole pattern shift on my ceramic board, rather than a few holes?

That is the signature of the green-forming route. Sintering shrinkage is a whole-sheet behaviour; formed dimensions are made oversized and the final size is set by shrinkage. If shrinkage is uneven across the sheet, the deviation appears as a systematic positional shift or distortion rather than random single-hole error. The fix direction is to re-confirm the hole-location datum — board edge or an on-board datum feature — so the deviation falls where you can accept it.

Q3: My drawing gave outline dimensions and tolerance. Why was it still rejected on edge condition?

Because dimension and edge condition are two different things. Ceramic edges fail by losing material (chipping), not by gaining it (burr), and a chip-out cannot be removed by post-processing. If the edge will later mate to a heat sink surface, enter a fixture or carry clamping load, the edge requirement must be stated on the drawing. Otherwise the factory ships to common practice and the customer rejects against assembly needs — both working from their own premise, which was never aligned.

Q4: Can ceramic boards be V-cut?

Essentially not. V-cut works by scoring then snapping, and snapping a brittle material means an uncontrolled crack path and an unguaranteeable broken face. Laser separation is the main method on ceramic, with dedicated abrasive routing viable in some cases; punching only works in the green state. This means the panelisation scheme cannot be copied from conventional material, and sometimes the conclusion is single-piece machining.

Q5: Why won't the factory just tell me the minimum hole size and location tolerance?

Because neither is an independent constant. Both are coupled to material type, substrate thickness and forming route: the same hole size is not equally viable on the green route and the post-sinter laser route, and not equally viable at different thicknesses. What a factory can give is a review conclusion for your specific board, not a number table that transfers across build types.

Q6: At design stage, what must I at least settle first?

Four things: which hole positions are critical and what they are referenced to; what function each outline edge serves later; whether the board has features that can only be defined after sintering; and whether single-piece delivery is acceptable. All four are information only the designer holds. Missing any one of them, a review can only return an answer carrying assumptions.

Related links

Need Professional PCB Manufacturing?

Founded in 2009, we provide one-stop PCB solutions from prototype to mass production.