A dark line in a microsection may be a product discontinuity, preparation damage or an optical effect at an uneven surface. Its colour alone cannot settle the question. Equally, an unexplained feature must not be dismissed as a polishing artifact simply because that explanation would permit acceptance.
This article addresses preparation-related uncertainty, not acceptance limits. For sampling and the broader purpose of sectioning, see PCB microsection analysis and acceptance. Product disposition remains subject to the drawing, applicable specification and approved decision procedure.
Preserve the first image before improving the surface
Retain the original image and identify the sample, board or panel location, section orientation and thermal-stress condition. Record preparation history, whether the surface was etched, image magnification and a valid scale. Keep an overview that locates the detailed image. Enlarging an uncalibrated photograph does not make it a dimensional measurement.
The first image matters because further preparation removes material. A later photograph may show another plane through the structure, not a repeat observation of exactly the same location. Keeping only the final attractive image can erase the evidence needed to explain the original finding.
Similar appearances can have different causes
| Observation | Preparation issue to investigate | What it does not prove |
|---|---|---|
| Similar-direction lines cross copper and resin | Residual grinding scratches or abrasive contamination | A shared direction does not establish that every line is a scratch |
| A copper edge has a tail or appears to bridge a gap | Soft copper smeared across the surface during preparation | Apparent continuity does not establish an intact original interface |
| A pit, debris or irregular dark region appears locally | Particle pull-out, embedded abrasive or inadequate edge support | A cavity may be an artifact, a product feature, or involve both |
| An edge looks rounded or interfaces cannot be focused together | Edge rounding or differential removal producing surface relief | A blurred boundary is not a sound thickness datum |
These are investigative clues, not image-only classification rules. A real crack can run near the polishing direction. Preparation can also extend damage along an already weak interface, so “artifact” and “product weakness” are not necessarily mutually exclusive explanations.
Re-polishing changes the evidence as well as the appearance
Where preparation is suspect, qualified personnel should select a controlled cleaning, re-polishing or re-sampling method. Define the question before removing more material. Preserve staged images and record how the observed plane changed. Etching can reveal some interfaces, but stronger contrast is not automatically a more faithful boundary; identify the treatment state in comparisons.
If a line disappears, the new plane no longer shows that line. A scratch may have been removed, but a local real defect may also have been passed during material removal. Persistence is not conclusive either: contaminated abrasives or an unsuitable preparation method can reproduce a similar mark.
The objective is therefore not to polish until a suspect feature vanishes. If edge rounding prevents reliable boundary identification, restore a valid surface or prepare another sample rather than selecting a favourable reading from a diffuse edge.
Use independent sections when the original plane cannot resolve the question
A neighbouring section or a different orientation may help test an explanation. Record its spatial relationship to the initial feature and, when necessary, prepare a new mount. A clean section somewhere else is evidence about that location; it does not establish that the original discontinuity never existed. Even another hole on the same panel may not reproduce a local condition.
Other evidence has its own limits. Electrical continuity can coexist with a local interface separation that still makes contact. A process log without an alarm does not establish that a visible anomaly must be a preparation artifact. Select supplementary checks for the suspected mechanism and project requirements, rather than requiring the same test package for every dark line.
Separate observation, interpretation and disposition
- Observation: location, preparation state and traceable images.
- Interpretation: evidence supporting a scratch, smearing or genuine separation, together with remaining alternatives.
- Limitations: material removed and original features no longer available for examination.
- Disposition: approved further sampling, containment, acceptance or other action. “Suspected artifact” is not synonymous with “confirmed conforming.”
Use quality assurance to review the inspection context. For a particular structure, submit the drawing revision, original images, sampling map and preparation history through engineering contact, alongside the relevant manufacturing capabilities. This is not a report of an SKPCB customer failure and does not prescribe universal polishing settings.
FAQ
Does a line crossing both copper and resin have to be a scratch?
No. It is a reason to investigate preparation direction and surface condition, not a definitive classification.
Can a board be accepted because the line disappeared after polishing?
Not on that observation alone. Material removal changed the plane and may have removed a local real feature. Document the change and follow the applicable disposition procedure.
Does a passing electrical test prove that a separation in the section is artificial?
No. The tests examine different attributes, and a local interface discontinuity may still conduct.
Can copper thickness be measured at a rounded edge?
Not reliably where rounding obscures the boundary needed for the measurement. A valid prepared plane or another sample is required.